Fracture of Zircaloy-4 cladding tubes with or without hydride blisters in uniaxial to plane strain conditions with standard and optimized expansion due to compression tests
Data and Resources
Additional Info
| Field | Value |
|---|---|
| Source | ISSN: 0921-5093 |
| Author | Hellouin de Menibus, Arthur, Auzoux, Quentin, Mongabure, Philippe, Macdonald, Vincent, Le Jolu, Thomas, Besson, Jacques, Crépin, Jérôme |
| Maintainer | CCSD |
| Last Updated | May 5, 2026, 20:34 (UTC) |
| Created | May 5, 2026, 20:34 (UTC) |
| Identifier | hal-00966156 |
| Language | en |
| Rights | https://about.hal.science/hal-authorisation-v1/ |
| contributor | Centre des Matériaux (MAT) ; Mines Paris - PSL (École nationale supérieure des mines de Paris) ; Université Paris Sciences et Lettres (PSL)-Université Paris Sciences et Lettres (PSL)-Centre National de la Recherche Scientifique (CNRS) |
| creator | Hellouin de Menibus, Arthur |
| date | 2014-05-05T00:00:00 |
| harvest_object_id | 371d0cbd-2da3-44c1-8b25-f8e8eac26f37 |
| harvest_source_id | 3374d638-d20b-4672-ba96-a23232d55657 |
| harvest_source_title | test moissonnage SELUNE |
| metadata_modified | 2025-12-01T00:00:00 |
| relation | info:eu-repo/semantics/altIdentifier/doi/10.1016/j.msea.2014.02.075 |
| set_spec | type:ART |